- Details
- By Super Admin
- Category: yuhejinfen
- Hits: 528

Application
Suitable for small sintered saw blades, medium-diameter saw blades for medium-soft granite, and mining segments.

Powder Morphology
The distribution of the product under high and low magnification microscopes, it shows the morphology of the powder.
- Details
- By Super Admin
- Category: yuhejinfen
- Hits: 500

Application
Suitable for all kinds of diamond tools, including sintered saw blades, medium diameter saw blades, segments of large diameter mining saw blades, grinding discs and blocks, chamfering wheels, etc

Powder Morphology
The distribution of the product under high and low magnification microscopes, it shows the morphology of the powder.
- Details
- By Super Admin
- Category: yuhejinfen
- Hits: 1141

Application
Suitable for the wear-resistant tools, such as concrete saw blades, wall grooving saw blades, grinding discs, grinding blocks, chamfering wheels, etc.

Powder Morphology
The distribution of the product under high and low magnification microscopes, it shows the morphology of the powder.
- Details
- By Super Admin
- Category: yuhejinfen
- Hits: 488

Application
Suitable for steel-concrete drill bits, steel-concrete saw blades, large cutter heads, grinding wheels, grinding blocks, wire saws, gang saws, etc.

Powder Morphology
The distribution of the product under high and low magnification microscopes, it shows the morphology of the powder.
- Details
- By Super Admin
- Category: yuhejinfen
- Hits: 1080

Application
Widely used in various diamond tools. Suitable for low hardness and high grades diamond tools. Such as wall grooving blades , small saw blades for soft rock and grinding tools.

Powder Morphology
The distribution of the product under high and low magnification microscopes, it shows the morphology of the powder.